الوصف
1, will need to
weld the pipe into the same type of fixture, the clamp;
2, the pipe ends with a dresser milling.
In the milling side, avoid too much force at both ends, to be
slowly repaired, to ensure the welding surface of the flat, when
there is a continuous cutting (basic milling the surface at both
ends), dropping the dresser, by adjusting the tightness of the
fixture (if necessary, turn the pipe) to calibration of two
docking tube, so that dislocation is not greater than *0% of wall
thickness;
3, heating the pipe with a heating plate.
The heating temperature raised to **0℃, when the set temperature is
reached, it will place the clamps on both ends of the heating
plate surface between the ends of the pipe to the heating plate
heating surface pressure, when both ends of the flange surface
pressure to a certain amount of 1.**2mm should stop the pressure,
heat-absorbing state for *0 seconds
4, docking
To endothermic time, remove the heating plate Xu Su, the both
ends of the face then pressed to make ends face the pressure
until there is about 3mm flange, release the handle.
5, cooled to ambient temperature, removable fixture.
بلد: |
China |
نموذج رقم: |
63-200
|
سعر فوب: |
(قابل للتفاوض)
أحصل على آخر سعر
|
الموقع: |
- |
سعر الحد الأدنى للطلب: |
- |
الحد الأدني للطلب: |
- |
تفاصيل التغليف: |
wooden box |
موعد التسليم: |
- |
القدرة على التوريد: |
- |
نوع الدفع: |
- |
مجموعة المنتج : |
welding machine
|