Description
CERBACK Brand Ceramic Welding back
up tapes & strips for one side welding. These are used for ALL
kind of WELDING PROCESSES & for ALMOST ALL METALS, for One Side
welding. Welding processes such as SMAW, FMAW, GMAW, SAW, CO2, TIG,
MIG etc.
Weld back up tape consists various
profiles of Non Porous CERAMIC tiles for butt welding, Fillet
welding etc.
We also manufacture SIBACK -
FIBERGLASS Backing Tapes.
SIBACK is a
high heat resistant aluminum backing tape with a woven fiberglass
having RED Center line for easy location in root gap
adjustment.
Very simple &
easy to use. Just peel off release paper from Aluminum. Stick
Aluminum tape to backside of the root gap on sheet, plate,
pipe or vessel, adjusting center line with Center of Root
gap. The fiberglass, which is One inch wide, covers the
root gap and leaves no open air gap, causing NO OXIDATION
.
By using fiberglass
weld back up tapes, Welding COST is saved approx *0 to *0% whereas
welding TIME is saved by *0%. RESULTS are **0% RADIOGRAPHIC
WELDING. No Back CHIPPING, No Back GRINDING or Gouging, No PURGING
required.
fiberglass welding
back up tapes are one inch in width, pasted at center of *5
mm wide Aluminum tape coated with temperature resistant acrylic
adhesive.
Fiberglass backing
tapes are available in *0mil (1 mm) thick, *0 Mil (1.5mm) thick
& **0 mil(3mm) thick.
By
using Weld back up
tapes,
- Increases productivity, Root weld and fill in one
pass
- Ideal for stainless steel and alloyed metals,
sheet, plate, pipes and vessels.
- Imparts X-ray quality back beads on root
pass.
- Saves argon gas as
no purging will be necessary, resulting Massive purge
gas savings. Makes process faster as it
saves time in preparation and assemble.
- Welds one side only.
- Provides incombustible, high temperature stability.
More flexible, low thermal conductivity, good thermal
shock resistance, good mechanical and chemical agents
resistance, good electrical properties.
- Saves cleaning costs.
- Eliminates weld defects, No re-welding &
re-work.
- For horizontal and vertical
welding.
- No Gouging or Grinding, Back
chipping.