HDPE VIRGIN RESIN Solid Insulation Compound

HDPE VIRGIN RESIN Solid Insulation Compound

( Negotiable )

|

Minimum Order

Place of Origin:

-

Price for Minimum Order:

-

Minimum Order Quantity:

10 Bag

Packaging Detail:

25 KG PER BAG

Delivery Time:

15 DAYS

Supplying Ability:

100 Bag per Week

Payment Type:

T/T

الاتصال الآن
عضو مجاني

الشخص الذي يمكن الاتصال به EMMA

Changchun, Jilin

الاتصال الآن

Description

High Density Polyethylene Solid Insulation Compound NT-7547
 HDPE NT-754is a high-molecular weight, high-density polyethylene insulation compound specifically formulated toprovide excellent oxidative stability, toughness, and abrasion resistance. It provides superior long term aging performance, while providing excellent environmental and thermal stress-cracking resistance.
In addition,HDPE NT-7547provides excellent processability for high-speed wire insulating extrusion processes.
 
Physical Nominal Value (English) Nominal Value (SI) Test Method
Density 0.947 g/cm³ 0.947 g/cm³ ASTM D792
Melt Mass-Flow Rate (190°C/2.16 kg) 0.75 g/10 min 0.75 g/10 min ASTM D1238
Environmental Stress-Cracking Resistance
212°F (100°C), 100% Igepal, F0
 
> 48.0 hr
 
> 48.0 hr
ASTM D1693
Mechanical Nominal Value (English) Nominal Value (SI) Test Method
Tensile Strength 3400 psi 23.4 MPa ASTM D638
Tensile Elongation (Break) 500 % 500 % ASTM D638
Thermal Nominal Value (English) Nominal Value (SI) Test Method
Brittleness Temperature -105 °F -76.0 °C ASTM D7461
Thermal Stress Crack Resistance - F0 > 4.0 day > 4.0 day ASTM D2951
Aging Nominal Value (English) Nominal Value (SI) Test Method
Retention of Tensile Elongation - 48 hrs
212°F (100°C)
 
90 %
 
90 %
ASTM D638
Retention of Tensile Strength - 48 hrs
212°F (100°C)
 
90 %
 
90 %
ASTM D638
Electrical Nominal Value (English) Nominal Value (SI) Test Method
Volume Resistivity (73°F (23°C)) > 1.0E+15 ohm·cm > 1.0E+15 ohm·cm ASTM D257
Dielectric Constant (1 MHz) 2.32 2.32 ASTM D15312
Dissipation Factor (1 MHz) 0.000060 0.000060 ASTM D1531
Extrusion Nominal Value (English) Nominal Value (SI)
Melt Temperature 425 to 500 °F 218 to 260 °C
Extrusion Notes
image

HDPE NT-7547provides excellent surface finish and good output rates over a broad range of extrusion conditions.HDPENT-7547is typically extruded at melt discharge temperatures ranging from 218-260°C (425-500°F) using conductor preheats ranging from 110-140°C (230-290°F). Specific extrusion conditions can be recommended only when the application, processing speed and processing equipment details are known.